http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H111344-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_88fbcd2a70a3c49d0aed69a000d55909 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-87 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C19-00 |
filingDate | 1997-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c4cc926f9af76d87f2acfc8cccc76919 |
publicationDate | 1999-01-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H111344-A |
titleOfInvention | Rib forming method |
abstract | (57) 【Abstract】PROBLEM TO BE SOLVED: To provide a good rib forming method using a ceramic material. A rib-forming ceramic material layer is provided with a photosensitive resin composition layer, and a predetermined recess is provided by exposure and development, the rib-forming ceramic material in the recess is removed, and then the rib is fired. 400 by the thermobalance of the photosensitive resin composition (measurement start temperature: 30° C., temperature rising rate: 5° C./min, measured in an air atmosphere). Weight loss rate at ℃ (WR 400 ) and weight loss rate at 600 ℃ (WR 600 ), and weight loss rate at 400 ℃ (W) C 400 ) and the weight loss rate at 600° C. (WC 600 ) are set to satisfy the relationship of (WR 400 /WR 600 )>(WC 400 /WC 600 ). |
priorityDate | 1997-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |