http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11133660-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fb9f44db08d1c42a53f3d28eaae416f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 1997-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f75f32e8d95b4f7b32e8d7097bc185cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9fd4bfc4c50c37c469c654f146db6339 |
publicationDate | 1999-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11133660-A |
titleOfInvention | Manufacturing method of toner |
abstract | (57) [Problem] To provide a method for producing a toner excellent in dispersibility of a colorant by a simple process. SOLUTION: 1) a step of stirring and mixing raw materials containing a binder resin and a colorant, 2) a step of melt-kneading the mixture obtained in step 1), and 3) a pulverization and classification of the melt-kneaded product obtained in step 2). In the method for producing a toner having the respective steps of step 1), in step 1), the temperature of [the temperature lower by 5 ° C. than the glass transition point (Tg) of the binder resin used] to [softening point (Tm) of the binder resin] A method for producing a toner, comprising stirring and mixing a binder resin and a colorant in a temperature range. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-100418013-C http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0169325-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6992150-B2 |
priorityDate | 1997-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 91.