http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11130890-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-06 |
filingDate | 1997-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a122dc7633929c7f9c3ba0b8061b76ad |
publicationDate | 1999-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11130890-A |
titleOfInvention | Olefin resin crosslinked foam |
abstract | (57) [Summary] [PROBLEMS] To produce a crosslinked olefin resin foam having excellent vacuum moldability and hot stamping moldability using a crosslinked olefin resin powder, and re-use this for automobile interior parts and the like. Use. SOLUTION: The gel fraction is 70 to 100% in an olefin resin crosslinked foam comprising an olefin resin mixture comprising 40 to 90% by weight of a propylene resin and 60 to 10% by weight of an ethylene resin, and Average particle size is 0.0 The crosslinked olefin resin powder having a particle size of 1 to 50 μm is used in an amount of 5 to 50 parts by weight based on 100 parts by weight of the olefin resin mixture. It is characterized by being dispersed by weight. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006052264-A |
priorityDate | 1997-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 40.