http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1112450-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_32681f1832d227fe8df23d12a37f67a8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 |
filingDate | 1998-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_031d7dea6d678cd775dcbd15b1c7444d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4ba549319eb2cbf2750a07053affcde6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7f9f23f125feca2ed495d56e38d384dc |
publicationDate | 1999-01-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1112450-A |
titleOfInvention | Antifouling thermoplastic composition |
abstract | PROBLEM TO BE SOLVED: To use a polyester resin which has a sufficient hardness and a long-term hot water resistance at the same time that a surface thereof has extremely excellent antifouling properties when a molded body is produced. Provision of a thermoplastic composition. SOLUTION: In addition to a thermoplastic polyester resin, an epoxy resin having an average epoxy equivalent of 80 to 1,000, and a curing accelerator used in the epoxy resin, the thermoplastic polyester resin and the epoxy resin further have an epoxy group. A resin having a resin or epoxy group incompatible with both resins and a resin having a specific gravity difference from the thermoplastic polyester resin in the range of 0.1 to 1 is blended. |
priorityDate | 1997-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |