http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11116949-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_796c8f26764fcde526e6ed4ec7952d0b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 |
filingDate | 1997-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2ef669035f927b7d48b7de231b10652b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e30abd2c2026b80e6d4e2627d6274445 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_384c56cbd2954921f81b7e11edd1c3d6 |
publicationDate | 1999-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11116949-A |
titleOfInvention | Liquid antioxidants and organic polymer materials containing them |
abstract | (57) [Summary] [PROBLEMS] When adding an antioxidant to prevent deterioration of an organic polymer material which is deteriorated by oxidation, heat and light, Either emulsification, dispersion, or suspension in an organic solvent or the like, or once melting and addition at a high temperature, requires a special operation, and a simpler addition method has been demanded. SOLUTION: Based on an organic material, 1 to 80% by weight of methyl 3- (3-tert-butyl-4-hydroxy-5-methylphenyl) propionate is added to 3- (3-tert-butyl-methyl) propionate. Room temperature containing 99% to 20% by weight of 2-ethylhexyl 4-hydroxy-5-methylphenyl) propionate and / or isotridecyl 3- (3-tert-butyl-4-hydroxy-5-methylphenyl) propionate By adding a liquid antioxidant, a stabilized organic polymer material can be obtained without any special operation, and the problem described above can be solved. |
priorityDate | 1997-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links