http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11107037-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-84 |
filingDate | 1997-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_be93254ab72c75f75065d7fb21356118 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_daf2a1c8592bd3c142bb18e14adf5e9c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_adc061c0dccfff39419ae3a283890273 |
publicationDate | 1999-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11107037-A |
titleOfInvention | Polyester fiber excellent in dimensional stability and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a high-strength polyester fiber excellent in dimensional stability and to improve the spinnability and drawability in a high-speed spinning-drawing method and to reduce yarn breakage. Provide a stable production method. SOLUTION: This is a fiber made of a polyester having an intrinsic viscosity of 0.7 or more and having substantially no branched structure and having an intrinsic viscosity of 0.7 or more and having ethylene terephthalate as a main repeating unit and having a crystallization temperature of 210 ° C. or more at a temperature drop of 6 g / d. It has a breaking strength of not less than 7 g / d and preferably a breaking elongation of not less than 12% and not less than 10 g at room temperature. % Polyester fiber having excellent dimensional stability and a method for producing the same. |
priorityDate | 1997-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |