http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11100559-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b051f9f7933c758e66f6ceda5c9fb2cc |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L29-04 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J123-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J131-04 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J131-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F218-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-24 |
filingDate | 1998-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5d01f174c1d887fe7deae6087adb9d0e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f0adf016e11fd56d8d50ceb9af36178 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bb6101af9ae4837322a8a90cf4614e2c |
publicationDate | 1999-04-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11100559-A |
titleOfInvention | Adhesive for difficult-to-join surfaces |
abstract | PROBLEM TO BE SOLVED: To provide an improved aqueous emulsion vinyl acetate for use in packaging applications and on difficult-to-join surfaces such as polyethylene, poly (ethylene terephthalate) and oriented polypropylene Providing an ethylene (VAE) polymer adhesive; The VAE polymer comprises about 55 to 80 wt% vinyl acetate, based on the total weight of the monomers. It contains one or more additional monomers that are copolymerizable with 15 to 45 wt% ethylene and 0 to 30 wt% ethylenically unsaturated. The cast film of the VAE emulsion polymer of the present invention has the following data points: 1 × 10 5 and 2 × 10 7 dynes / cm at 23 ° C. 2 and 1 × 10 3 and 2 × 10 6 dynes / cm 2 at 70 ° C. Between 1 × 10 6 and 1.5 × 10 7 dynes / cm 2 at 23 ° C., and 3 × 10 4 at 70 ° C. And a tensile storage modulus in the region between 9 × 10 5 dynes / cm 2 (test frequency 6.28 radians / cm 2 ). Seconds). |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2022523085-A |
priorityDate | 1997-07-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 63.