http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1095884-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 |
filingDate | 1996-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8e339d27ecffbb8a06b4729340ad74bc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a12ffdadf0a2ee9a3ba978ce441b535e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6eb223608718042c76e2c830d885b2d9 |
publicationDate | 1998-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1095884-A |
titleOfInvention | Resin composition and laminate using the same |
abstract | (57) [Problem] To provide a resin composition excellent in extrusion or injection melting property and useful as an adhesive between a polyolefin resin layer and a fluorine resin layer or an acrylic resin layer. SOLUTION: 100 parts by weight of an acrylic graft copolymer (A) obtained by the following production method are mixed with an olefin resin (B) 1 to A resin composition comprising 150 parts by weight and 1 to 150 parts by weight of an acrylic resin (C), wherein the sum of the components (B) and (C) is 170 parts by weight or less. Acrylic graft copolymer (A): A radical polymerizable monomer (b) having a functional group reactive with the olefin resin (a) having at least one functional group in one molecule. The reaction is carried out to obtain a radically polymerizable olefin resin (c), and alkyl acrylate or alkyl methacrylate (the alkyl group having 1 to 8 carbon atoms) is added to 100 parts by weight of the resin (c). An acrylic graft copolymer obtained by subjecting (d) to radical copolymerization at a ratio of 10 to 500 parts by weight. |
priorityDate | 1996-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |