Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_696ca0ae93d5cf5a686273601361781f |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23G5-032 |
filingDate |
1996-06-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_196b6d2d0f380bafbe47dd2b988efcbd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01f19c46707dc43619f7b03f17a4304e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b48c772dd9ef0e3aafc7830bec5346c6 |
publicationDate |
1998-01-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H108278-A |
titleOfInvention |
Metal drying method |
abstract |
(57) [Problem] To provide a drying method for preventing drying unevenness and spots in the field of aqueous metal surface treatment and metal cleaning. SOLUTION: After treatment with a metal surface treatment agent or a metal cleaning agent, and then with a treatment agent comprising an aqueous solution containing acetylene alcohol having 3 to 10 carbon atoms, drying without washing with water. Characteristic metal drying method. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20110088496-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8420529-B2 |
priorityDate |
1996-06-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |