http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H107882-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e8b42c9a345a988783d1ed1d06565f17 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-04 |
filingDate | 1996-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_94a7dfdc70b7d43cfc697259a8dc73a9 |
publicationDate | 1998-01-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H107882-A |
titleOfInvention | Fiber reinforced composite material |
abstract | PROBLEM TO BE SOLVED: To produce a fiber-reinforced composite material by curing a fiber using a phenolic resin as a matrix material, and to use an acid curing agent to uniformly degrade the fiber without causing deterioration of the fiber. It is an object of the present invention to provide a composite material which can be formed by curing, has excellent room temperature strength, has excellent alkali resistance and heat resistance, and can be effectively used as a substitute for a reinforcing bar or the like. SOLUTION: The preferred composite material as described above is obtained by mixing a sulfonic acid curing agent having a certain range of acid value in a fiber and a phenolic resin, a fiber deterioration inhibitor, ultrafine silica, and further, if necessary, a filler. be able to. |