http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1060423-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E70-30 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F28D20-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-44 |
filingDate | 1997-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e33ebf09056c8dc1953d1ec2f5b5031 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3dc3644c881a28a81a35466136540c51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_335408da76a7c83e0f93dd111dd60f12 |
publicationDate | 1998-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1060423-A |
titleOfInvention | Method of manufacturing heat storage agent and method of manufacturing heat storage material |
abstract | PROBLEM TO BE SOLVED: To provide a highly safe heat storage agent which prevents leakage due to fluidization of an oily substance such as paraffin having flammability and heat storage property and avoids leakage due to deterioration over time. And a heat storage material using the same at low cost and stably. A monomer component is polymerized in the presence of an oily substance having a heat storage property, and in a polymer obtained by polymerizing the monomer component, the fluidity of the oily substance that liquefies due to phase change is reduced. By keeping the oily substance in a gel or solid state so that leakage of the oily substance due to deterioration over time is reduced, the heat storage agent excellent in physical properties and safety, and the polymer are placed in a container. By forming the heat storage agent tightly in the container, the heat storage material with improved thermal efficiency is stably formed, And it is manufactured at low cost. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010249412-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005097543-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006132914-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4617106-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3623422-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004168792-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11352466-B2 |
priorityDate | 1996-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 96.