http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1045956-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ba6b0846b5959035d7b470d804bcca0f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C409-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 |
filingDate | 1996-08-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9d9132ade5cc72bed89561b74f40bdaa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aa68dd573abc997d4fd40ab9e75dd72a |
publicationDate | 1998-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1045956-A |
titleOfInvention | Organic peroxide formulations |
abstract | (57) Abstract: A polyolefin resin powder or pellet 25 having a fine pore structure having a pore diameter of 0.05 to 10 μm. 75% by weight of liquid or powdery organic peroxide at room temperature A compound of an organic peroxide, which is blended with 10 to 10% by weight. The organic peroxide composition of the present invention contains a large amount of organic peroxide, so that only a small amount is required for modifying a polyolefin resin using the organic peroxide. The clogging inside is improved, and the variation in the reforming effect due to the volatilization of the organic peroxide can be reduced. These effects make it possible to reduce the cost and stabilize the process of modifying the polyolefin resin using an organic peroxide. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100597450-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8329808-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011513545-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006137849-A |
priorityDate | 1996-08-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 80.