http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1043834-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fb9f44db08d1c42a53f3d28eaae416f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C1-22 |
filingDate | 1997-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cb3efd027fa3c686ff6fb17bfbf056e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f0e8ee2728e56cb548f9e648e0b7ce9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_adccd499235ff2d086ddb14f00d4e54c |
publicationDate | 1998-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1043834-A |
titleOfInvention | Binder composition for curing carbon dioxide |
abstract | (57) [Problem] To improve the pot life of a mold composition for curing carbon dioxide gas and the strength of the obtained mold. SOLUTION: In a binder composition used in a mold production method of curing an aqueous solution of a water-soluble phenolic resin with carbon dioxide, the water-soluble phenolic resin has the following properties. Binder composition, A mold composition for curing carbon dioxide containing the same, and a mold making method using the same. (A) The weight average molecular weight is 500 to 6000 (b) The molar ratio of aldehyde to the total number of moles of phenols and / or bisphenols is 1.0 to 3.0. (C) The alkali metal relative to the total number of moles of phenols and / or bisphenols The molar ratio of hydroxide is 0.5 to 4.0 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0574930-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0574930-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190025686-A |
priorityDate | 1996-05-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 145.