Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L47-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-01 |
filingDate |
1996-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5349ae2faf49ccfa3dfe2a9c49cb2e19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c7a21e2df288ba0cadef2555542ae1b0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_deda2d100c181161740b3cd78e9e4c29 |
publicationDate |
1998-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H1036595-A |
titleOfInvention |
Low hardness rubber composition and vibration absorbing material |
abstract |
(57) [Problem] To provide a low hardness rubber composition and a vibration absorber excellent in flexibility. SOLUTION: An ethylene / α-olefin / non-conjugated diene copolymer rubber 10 having the following characteristics (a) to (e): A low-hardness rubber composition comprising 0 parts by weight and 50 to 150 parts by weight of a softener. (A) carbon number of α-olefin: 4 or more and 20 or less; (B) α-olefin content: 50 mol% to 90 mol%, (c) Mooney viscosity at 100 ° C .: 40 to less than 200, (d) iodine value: 3 to 50, (E) Molecular weight distribution: 3 or less |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2866309-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6632541-B2 |
priorityDate |
1996-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |