http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10338563-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-27 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-101 |
filingDate | 1997-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_213bbfa3eddce459450070b1e1b37c91 |
publicationDate | 1998-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10338563-A |
titleOfInvention | Method for producing inorganic composition and inorganic molded product |
abstract | (57) [Problem] To provide an inorganic molded product excellent in strength such as bending strength and water resistance. SOLUTION: A fatty acid ester compound is contained in an amount of 0.01 to 15 parts by weight in a hydraulic composition composed of calcareous powder, siliceous powder and reinforcing fibers, or a vinyl alcohol-based polymer is added thereto in an amount of 0.01 to 15 parts by weight. .05 to 1 Molding an inorganic composition containing 0 parts by weight, and after primary curing, autoclaving at 120 to 200 ° C. to obtain an inorganic molded product. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006103675-A1 |
priorityDate | 1997-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 62.