http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10325016-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9e1bf06f55de84b78abc9a057807f7eb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-90 |
filingDate | 1997-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e035282525e173927a7efb3ee5ac4d4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_860d5bc96c5e2b6e33966adc5bae7862 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3aba53b210c3bd72f22adb606e224d1f |
publicationDate | 1998-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10325016-A |
titleOfInvention | Moisture and heat resistant polyester filament and its manufacturing method |
abstract | (57) [Problem] To provide a polyester filament which does not fibrillate, has good thread properties, and maintains excellent wet heat resistance for a long period of time, and a method for producing the same. SOLUTION: 75% by weight or more of polyester produced through a solid-state polymerization reaction, 0.1 to 20% by weight of a copolymer of ethylene and glycidyl methacrylate (and 0.1 to 0.1% of polyolefin) -20% by weight) and a filament obtained by melt-spinning and stretching a composition comprising 0.3 to 2.0% by weight of a carbodiimide compound having a relative viscosity of 1.40 or more and a carboxyl end group amount of 10.0 eq / t or less. Some polyester filaments. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006233375-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002030208-A |
priorityDate | 1997-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 42.