http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1031818-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_294881271413951a95f284b588a68e66 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-842 |
filingDate | 1996-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f49cc0a0ecbcf4e5a92a0fe8d089b49d |
publicationDate | 1998-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1031818-A |
titleOfInvention | Manufacturing method of magnetic recording medium |
abstract | (57) [Problem] To manufacture a magnetic recording medium having a lower non-magnetic layer magnetic layer by a wet-on-wet coating method so that a lower upper layer interface and an upper magnetic layer surface can be formed in a good state. I do. SOLUTION: A complex elastic modulus G * of a magnetic paint for an upper layer is defined as a time 0 second immediately after an initial shear of 60% at a strain of 1000% and an angular velocity of 2πrad / sec. Complex elastic modulus G * at 1% strain and 2πrad / sec angular velocity (0) and a complex elastic modulus G at a strain of 1% and an angular velocity of 2πrad / sec at a time point when 120 seconds have elapsed from time 0 seconds. * (120) is G * (0) / G * (120) ≦ Set so as to satisfy the condition of 3.0. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2016084718-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016084718-A1 |
priorityDate | 1996-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 45.