http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10316731-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0cdb395105a75f1b0346cc31b81fade1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G8-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-06 |
filingDate | 1997-05-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b32b4ec35ced607748840c58ee92be1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_105005710925df79a8050ef14b5c52de |
publicationDate | 1998-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10316731-A |
titleOfInvention | Resin composition for friction material |
abstract | (57) [Summary] [PROBLEMS] To reduce the time required for molding and firing in a friction material manufacturing process. SOLUTION: This is a polycondensate of a phenol and an aldehyde, wherein the ratio of the ortho bond to the para bond (o / p ratio) in the methylene bond in the resin is 0.7 or more and less than 1.0. And a hexamethylenetetramine as an essential component. |
priorityDate | 1997-05-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 66.