http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10292073-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_173b2b8743d9e7fb464fc1129186a5a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H3-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 |
filingDate | 1997-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_90f6f3528fce6c6a933d16f8050230f9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_63b031bb349418d6eeb33b7d0137fc33 |
publicationDate | 1998-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10292073-A |
titleOfInvention | Polypropylene resin composition for non-woven fabric |
abstract | PROBLEM TO BE SOLVED: To provide a polypropylene resin composition for a nonwoven fabric capable of producing a nonwoven fabric with low formation and good formation with high productivity at the time of spinning. SOLUTION: The polypropylene resin composition for a nonwoven fabric is obtained by mixing the following components (A), (B) and (C). Component (A): a crystal having a ratio (Mw / Mn) between the weight average molecular weight (Mw) and the number average molecular weight (Mn) of 2 to 4 and a melt flow rate (MFR) of 20 to 100 g / 10 minutes. Component (B): Spreader 0.03 to 0.3 parts by weight Component (C): One or more hydroxides of metals selected from Group Ia and Group IIa. 003 to 0.3 parts by weight |