http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10287751-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-08 |
filingDate | 1997-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_335eb584280c342f5a05fa2d2bf78d65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_990f02469e8ee15db152845e5cbc64ec |
publicationDate | 1998-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10287751-A |
titleOfInvention | Styrene resin molded product and method for producing the same |
abstract | (57) [Summary] [PROBLEMS] To have extremely excellent physical properties of syndiotactic polystyrene and isotactic polystyrene, Furthermore, to obtain a resin molded product having excellent moldability. SOLUTION: This is a molded article comprising a mixture of 55 to 95% by weight of crystalline polystyrene having a syndiotactic structure and 45 to 5% by weight of crystalline polystyrene having an isotactic structure, and crystallization of the molded article. A styrenic resin molded product characterized in that the temperature has a single peak, and a method for producing the same. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001294619-A |
priorityDate | 1997-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 49.