http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10279901-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_026917a1661e94c21035d1c5d1fa135e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-06 |
filingDate | 1997-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4149852db57fb654c8ab27c247b3ba61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ecf6c2262fe16eb521fdeea89f6c1e6 |
publicationDate | 1998-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10279901-A |
titleOfInvention | Adhesive sheet and method for producing adhesive sheet |
abstract | (57) [Summary] [Problem] To provide a pressure-sensitive adhesive sheet which has little discoloration due to ultraviolet rays, sunlight, fluorescent lamps, etc., does not crack or tear the substrate even after exposure to light, and has little change in adhesive strength. I do. A pressure-sensitive adhesive sheet comprising a pressure-sensitive adhesive layer laminated on a surface substrate, wherein the pressure-sensitive adhesive layer contains 60 to 99% by weight of a (meth) acrylic acid alkyl ester monomer having 4 to 18 carbon atoms (meth). An acrylic pressure-sensitive adhesive composition containing an acrylic acid copolymer as a main component, a (meth) acrylic acid copolymer 1 The ultraviolet absorber is used in an amount of 0.3 to 10 parts by weight of the active ingredient with respect to 00 parts by weight. In the case of a solid ultraviolet absorber, it is in the form of an organic solvent solution, and in the case of a liquid ultraviolet absorber, it is as it is. Or a pressure-sensitive adhesive sheet characterized by being coated with a coating solution for a pressure-sensitive adhesive layer containing the same in a form diluted with an organic solvent, and having a residual solvent concentration of 10 to 2000 ppm after drying of the pressure-sensitive adhesive layer. It is. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9359528-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019073702-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101724358-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011105878-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018168333-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011154700-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101293879-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008123334-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4548754-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101233149-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006045315-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101177912-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019069552-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008248131-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009009137-A |
priorityDate | 1997-02-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 127.