abstract |
(57) [Summary] [PROBLEMS] To provide a silver halide photographic light-sensitive material capable of achieving low replenishment, high processing stability, no generation of silver stain, and obtaining an image of good image quality. Provide a processing method. In A AgCl content of 20 mole% or more, 50% or more of the total silver halide grains in the projected area has a silver halide emulsion is a two or more tabular grain aspect ratio, one side 1 m 2 per Ag A photographic material having a coating amount of 1.5 g or less, a gelatin coating amount of 2.1 g or less, and a swelling ratio of 180% or less was used. A developing solution containing ascorbic acid as a developing agent was used. The processing is performed as follows (all per 1 m 2 of light-sensitive material) by an automatic processing machine. |