http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10264959-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-10 |
filingDate | 1997-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86f915fc573dea5e8e952db384490197 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14e59be2dc36f7c68ff4291b93ca20d5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_23dd7363d567ea14d229fd27cb0d2cbb |
publicationDate | 1998-10-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10264959-A |
titleOfInvention | Packing materials such as bottle lids |
abstract | (57) [Problem] To provide a packing material which is excellent in flexibility and elastic recovery power, has good heat resistance, and does not change the taste and smell of the contents. SOLUTION: A packing material such as a bottle lid contains a constituent unit derived from an aromatic vinyl compound at a ratio of 0.1 to 5.0 mol%, and a maximum peak in an endothermic curve measured by a differential scanning calorimeter. The temperature at the position (Tm) is 100 ° C. or higher, and the intrinsic viscosity [η] measured in decalin at 135 ° C. Is in the range of 0.1 to 10 dl / g. |
priorityDate | 1997-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links