http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10245797-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a8cde4f2bd60df7888c8040bdfcc8a5d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-10 |
filingDate | 1997-02-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4de827ace6361f9ef21d3ec6ef6eea96 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b3730e36b0057fb6dee591de675af53c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0dc77284f86461ac06447aae334cc0c9 |
publicationDate | 1998-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10245797-A |
titleOfInvention | Paper coating agent |
abstract | PROBLEM TO BE SOLVED: To provide a coating agent for paper having a high yield on a paper surface, a high effect of improving surface properties such as barrier properties and surface strength, and excellent in high-speed coating properties. SOLUTION: (A) When the saponification degree is 60 mol% or more, For 100 parts by weight of a polyvinyl alcohol-based resin having a 4% aqueous solution viscosity of 1.5 mPa · s or more at 0 ° C., the degree of substitution (B) is 0.05 or more and 4% at 20 ° C. % Aqueous solution having a viscosity of 1.5 mPa · s or more is mixed with 0.1 to 50 parts by weight of a phosphorylated esterified starch. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2005052255-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011236516-A |
priorityDate | 1997-02-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 43.