http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10244760-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be92719b856db86c092cc233e9512ca2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-333 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-00 |
filingDate | 1997-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6be54ae2e391434d29e7afd8d951cd1b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5defabd00bb7fd22a3e01a10a34805c4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ef01a8bf14d8a3b42b1b0ad5ca2ac9ac |
publicationDate | 1998-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10244760-A |
titleOfInvention | Thermal recording material |
abstract | (57) [Summary] (with correction) [PROBLEMS] To provide a thermosensitive recording material having high stability of recorded images and excellent storage stability. SOLUTION: In a heat-sensitive recording material having a heat-sensitive coloring layer mainly composed of a leuco dye and a color developing agent for coloring the leuco dye on heating on a support, the following general formula (1) is used as the color developing agent. The phenolic compound represented is used. (However, r in the formula represents an integer of 1 to 3, and R represents an aliphatic hydrocarbon group which may have a substituent.) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010024419-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8771912-B2 |
priorityDate | 1997-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 233.