http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10194816-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-20 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F257-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F271-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-04 |
filingDate | 1997-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6585f081c92780f4f5c0f3f17170ab37 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bdf554979f4a3ebda0adc920f7e3faf1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_575e8464a6012c420bbf227b9a6727b7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4aef7455be9b524f8ac3a6e93d7dc8df |
publicationDate | 1998-07-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10194816-A |
titleOfInvention | Cement composition |
abstract | (57) Abstract: A cement composition comprising a cement, an aggregate, and a (co) polymer as essential components, wherein the (co) polymer has at least one surface of a core by a shell. Wherein the core is a (co) polymer which is insoluble in water, and the shell is a (co) polymer which is water-soluble at a pH of 5 or more. A cement composition characterized in that it is a (co) polymer which can be substantially re-emulsified at a pH of 5 or more. A hardened cementitious product obtained by mixing water with the cement composition of the above and curing the mixture. Effect The cement composition according to the present invention has the following to It has excellent characteristics. Excellent in fluidity and fluidity stability over time when blended with water. The hardened cement obtained by mixing with water and hardening is excellent in adhesive strength, water resistance and water absorption resistance. It can be suitably applied to base adjustment materials, self-leveling materials, repair materials, tile adhesives, grout for semi-flexible pavement, cement-based siding materials, joint materials, sprayed mortar materials, cement-based thick coating materials, cement-based injection materials, etc. . |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002137948-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2007007675-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006233145-A |
priorityDate | 1997-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 180.