http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10182866-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 |
filingDate | 1996-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b633a2ac75c34b0cba628e4795136c58 |
publicationDate | 1998-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10182866-A |
titleOfInvention | Ethylene resin foam |
abstract | (57) [Problem] To provide a tough and flexible ethylene-based resin foam having a uniform cell shape and excellent appearance. A density in the range of 0.880~0.940g / cm 3, 1 MFR at 90 ° C, 2.16 kg load is in the range of 0.1 to 20 g / 10 min, and the decane soluble component amount ratio (W) and density (d) at room temperature are MFR ≦ 10 g / 10 min W <80 × exp (-100d-0.88)) + 0.1, M FR <10g / 10min W <80 × (MFR-9) 0.26 × exp (-100 (d-0. 88)) The relationship indicated by +0.1 is satisfied, and the relationship between the temperature (TM) and the density (d) at the maximum peak position of the endothermic curve measured by the differential scanning calorimeter is expressed by Tm <400 × d-250. An ethylene-based resin foam consisting of an ethylene-α-olefin copolymer to be filled. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000191848-A |
priorityDate | 1996-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 195.