http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10177234-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-35 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-305 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-30 |
filingDate | 1996-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50407473b316c18d520775bfb2b9e70c |
publicationDate | 1998-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10177234-A |
titleOfInvention | Silver halide photographic material and processing method thereof |
abstract | (57) [Summary] [Problem] To provide a silver halide photographic light-sensitive material having a low fog, no variation in running sensitivity and an excellent silver tone, and a processing method. SOLUTION: The support is provided with at least one photosensitive silver halide emulsion layer and a hydrophilic colloid layer, and a non-photosensitive hydrophilic colloid layer is provided on the side of the silver halide emulsion layer farther from the support. At least one layer selected from the silver halide emulsion layer and / or the hydrophilic colloid layer contains a leuco compound which reacts with an oxidized form of a developing agent to give a blue dye, and Wherein the pH of the outermost surface of the non-photosensitive hydrophilic colloid layer is not less than 7.0 and not more than 9.0, and the development of these silver halide photographic materials containing reductones. A method for processing a silver halide photographic material, comprising developing with a liquid. |