Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-02 |
filingDate |
1996-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ad06f72032612b7ada68ebe38a8a44ad http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_940df9fd6ca25f42d555c2e5433e9a00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9af32e9416b78e3a5429f2c85dc10fd8 |
publicationDate |
1998-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H10176122-A |
titleOfInvention |
Aqueous coating composition |
abstract |
PROBLEM TO BE SOLVED: To provide an aqueous coating composition excellent in film forming property, adhesion to a substrate, low-temperature flexibility and stain resistance. SOLUTION: An emulsion (A) in which a polymer obtained by polymerizing a vinyl monomer in an aqueous medium has a glass transition temperature of 40 to 80 ° C, and a vinyl monomer is polymerized in an aqueous medium. The glass transition temperature of the obtained polymer is -10 to 2 The emulsion (B) at 0 ° C is blended so that the glass transition temperature of the polymer in the emulsion is 25 to 50 ° C. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006526689-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3781622-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001181555-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009506186-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001081358-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7014990-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4818908-B2 |
priorityDate |
1996-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |