http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10176040-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-86 |
filingDate | 1996-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f0b1d40956a116f7341aed2df9a1e266 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_23773675a03fd06e4f4bd5774bed491c |
publicationDate | 1998-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10176040-A |
titleOfInvention | Method for producing polyester and polyester fiber excellent in moldability |
abstract | PROBLEM TO BE SOLVED: To provide a polyester having good thermal stability, less generation of sublimates at the time of melting, and improving the stability at the time of molding and the quality of the obtained molded product. SOLUTION: In an ethylene terephthalate-based polyester using an antimony compound as a polymerization catalyst, While adjusting the intrinsic viscosity (IV) of the polyester to 0.5 to 0.8, the concentration of terminal glycol groups (OH: equivalent / ton) And IV, the following expression is satisfied. OH ≦ 96.6 / IV-93.2 |