abstract |
(57) [Summary] Flame retardant PC / ABS containing fibrous filler Improve the appearance and fluidity of the alloy, as well as impact resistance, rigidity, To obtain a resin composition capable of providing a molded article with less warpage without lowering flame retardancy. SOLUTION: Polycarbonate resin (A) 30 to 80 Per 100 parts by weight of a composition consisting of 3% to 20% by weight of a saturated polyester resin (B) and 3 to 50% by weight of an ABS resin (C) per 100 parts by weight of a halogen-based flame retardant and / or a phosphorus-based flame retardant (D). A thermoplastic resin composition comprising 30 to 30 parts by weight and 1 to 30 parts by weight of a fibrous filler (E). |