abstract |
(57) [Problem] To provide a composition having smoke resistance and fire resistance. SOLUTION: (A) (i) Diorganosiloxane polymer 10 0 parts by weight and (ii) a crosslinking agent selected from linear aminooxy-functional siloxanes, cyclic aminooxy-functional siloxanes, aminooxy-functional silanes and partial hydrolysis products thereof A dispersed phase containing a product formed from a constituent material containing 0.1 to 20 parts by weight; (B) 50 to 300 parts by weight of water; (C) a surfactant selected from an anionic surfactant and a nonionic surfactant 0.5 to 10 parts by weight; and (D) 60 to 120 parts by weight of a filler selected from aluminum trihydrate, fumed titanium dioxide, zinc borate, magnesium oxide and ceramic filler, an aqueous solution forming an elastomer by dehydration. Silicone emulsion. |