Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-542 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A47C27-12 |
filingDate |
1996-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9d0118b54ddb3fbece51f2f368d2c396 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4112822e023af8a8441c08054252da18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ab9ab50fdcdc1b4d96918ddb630c1246 |
publicationDate |
1998-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H10117891-A |
titleOfInvention |
Fiber molded cushion material and method for producing the same |
abstract |
(57) [Problem] To provide a comfortable fiber cushion material excellent in cushioning property, air permeability and durability. SOLUTION: Apparent density of synthetic fiber material 0.0 In a molded cushion material having a thickness of 2 to 0.08 g / cm 3 and a hardness of 15 to 70 kgf, hollow holes having a length of 40% of the thickness are scattered in a thickness direction of the cushion material, A molded cushion material made of fiber, characterized in that the occupation ratio (volume ratio) of all the cavity holes in the cushion material is in the range of 2 to 40%. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7661764-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9038252-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9421895-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/GB-2441417-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7934774-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/GB-2441418-A |
priorityDate |
1996-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |