Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5d04736b0b882a4f5a1e0e0e4cd8cbb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C12R1-645 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C12N1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C12N1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-06 |
filingDate |
1996-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd4da1a8c55cca979faea6db165fe93d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_019253804150c5bf2196ef4db915ec66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6497848a3190f7ce7a153b73c8914f34 |
publicationDate |
1998-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H10117768-A |
titleOfInvention |
Decomposition method of aliphatic polyester resin and microbial preparation |
abstract |
PROBLEM TO BE SOLVED: To provide a method for rapidly decomposing an aliphatic polyester resin, particularly under a composting treatment condition, and a microorganism preparation therefor. SOLUTION: A method of decomposing an aliphatic polyester resin, which comprises contacting a microorganism having an ability to decompose polyester and having an optimum growth temperature of 40 ° C. or higher with the aliphatic polyester resin, preferably maintaining the temperature at 40 ° C. or higher, and a fat Microbial preparation for decomposing aromatic polyester resin. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002226624-A |
priorityDate |
1996-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |