http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10109391-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 |
filingDate | 1996-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2fe2a602a4e134c47e63cab8faae9b77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ae04d8ea62cee7d6f6beab9bac8f801 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2826f096e546745ccc5f3cec94d2df55 |
publicationDate | 1998-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H10109391-A |
titleOfInvention | Biaxially stretched laminated film for metal plate lamination |
abstract | (57) [Summary] [PROBLEMS] To provide excellent impact resistance at a low temperature, good taste retention, good adhesion to a metal plate, and also excellent film forming properties (extrudability, stretchability). For good metal plate lamination 2 An axially stretched laminated film is provided. SOLUTION: A first layer (A) made of polyester having ethylene terephthalate as a main repeating unit, 20 to 60% by weight of polycarbonate and 40 to 100% of polyester. 80% by weight of the composition, wherein the polyester comprises 10 to 90% by weight of a polyester having ethylene terephthalate as a main repeating unit and 10 to 9% by weight of a polyester having butylene terephthalate as a main repeating unit. A biaxially stretched laminated film obtained by laminating a second layer (B) of 0% by weight, wherein the first layer (A) of the film is subjected to an extraction treatment with pure water at 125 ° C. for 30 minutes. The biaxially stretched laminated film for metal plate lamination, characterized in that the extraction amount of the polymer is 2 × 10 −2 mg / cm 2 or less. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020010318-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11110688-B2 |
priorityDate | 1996-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 57.