http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0995820-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 |
filingDate | 1995-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d768b507c132194a868ff66eeea948ab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_18f4a83a05b82f3c25b1ce77f0a76d3c |
publicationDate | 1997-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0995820-A |
titleOfInvention | High shrink fiber |
abstract | (57) [PROBLEMS] To provide a polyester fiber having not only a high shrinkage property which has not been heretofore available but also a light resistance in a high speed spinning. A polyester fiber comprising a dicarboxylic acid component and a diol component, which is obtained by copolymerizing a compound having a norbornane skeleton, satisfies the following formula I, and has a breaking elongation of 90% or less. High shrink polyester fiber. 0.008 ≦ (WSr × A / B) ≦ 0.25 ... (I) [where WSr is the boiling water shrinkage rate (%) of the fiber, A is the copolymerization rate (%) of the above compound, and B is Indicates a spinning speed (m / min), and B ≧ 4500. ] |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6309719-B1 |
priorityDate | 1995-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |