http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0982354-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_345d74727e77e6d36988fd1168fb2589 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-28 |
filingDate | 1995-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6dd59d47add36bec6d5d1ed932377c58 |
publicationDate | 1997-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0982354-A |
titleOfInvention | Manufacturing method of alkaline secondary battery |
abstract | (57) [Problem] To provide an alkaline secondary battery having an improved charge / discharge cycle life. SOLUTION: A paste type positive electrode containing nickel hydroxide and a conductive agent composed of one or more kinds selected from metallic cobalt and a cobalt compound, a negative electrode, a separator interposed between the positive electrode and the negative electrode, and an alkali. A method of manufacturing an alkaline secondary battery provided with an electrolytic solution is characterized by storing for at least one month after initial charge and discharge. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006049149-A |
priorityDate | 1995-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 29.