abstract |
(57) Abstract: [PROBLEMS] To provide a resin composition and a molded article having an improved utilization rate by controlling the release (bleeding) of an active compound having a low transpiration property. SOLUTION: This resin comprises 100 parts by weight of a resin, 0.01 to 200 parts by weight of an active compound, and 0.1 to 100 parts by weight of a transpiration plasticizer having a vapor pressure of 0.001 mmHg or more at 20 ° C. The vapor pressure at 20 ° C. (P1) and the vapor pressure at 20 ° C. (P2) of the active compound have the formula: P A resin composition and a molded product satisfying 1 / P2 ≧ 2. |