http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0971610-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_afea2aa6f1f892c1456cf7d7a8bc0242 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-04 |
filingDate | 1995-09-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1755ec8dd520d0296522d506da28fbb5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a987f29a389d964d03567e432e6fe531 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dd371fbf109bb68f2ae6baedd2ac8394 |
publicationDate | 1997-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0971610-A |
titleOfInvention | Manufacturing method of polyolefin with wide molecular weight distribution |
abstract | (57) Abstract: [PROBLEMS] To provide a method for easily and easily producing a polyolefin having a wide molecular weight distribution, which is homogeneous and has an excellent balance of various physical properties such as melt elasticity, flow properties and mechanical properties. SOLUTION: The amount of hydrogen gas supplied to the slurry polymerization reactor is changed to three or more stages within the average residence time at a time interval of less than 1/2 of the average residence time in the polymerization reactor, while the solid catalyst component A method for producing a polyolefin having a wide molecular weight distribution, which comprises continuously polymerizing an olefin using a catalyst composed of an organometallic compound. |
priorityDate | 1995-09-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 123.