http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0970945-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41C1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41N3-00 |
filingDate | 1995-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f01dc304e87e487283cc679b71d8a55 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1f8be2ef9c3e1d8085b682cd7414206 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a20c82046af17d507a1e20811b38aca3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a885cc59719d2e8828ee75897b1e5c1d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_794631c736e46e56fd9b09edca0bc6b8 |
publicationDate | 1997-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0970945-A |
titleOfInvention | Method for producing support for photosensitive lithographic printing plate |
abstract | (57) Abstract: The present invention provides a method for producing a support for a photosensitive lithographic printing plate, which has good dot gain and stop stains and can be produced at low cost. The present invention provides a method for producing a photosensitive lithographic printing plate support in which an aluminum plate is mechanically roughened and then subjected to anodizing treatment, wherein the mechanical roughening is performed with a Mohs hardness of 8 or more. And using an abrasive having a mesh size of 600 to 1000, or performing the mechanical roughening with a Mohs hardness of 8 or more and a mesh size of 600 to 10 00 together with an abrasive having a Mohs hardness of 5 or more and less than 8 and a mesh size of 400 to 600, or the mechanical roughening is performed with an abrasive having a Mohs hardness of 8 or more. It is carried out by mixing with an abrasive having a hardness of 5 or more and less than 8 and the ratio of the abrasive having a Mohs hardness of 8 or more is 7 The range is 0% or more and less than 90%. |
priorityDate | 1995-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |