http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0954425-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-00 |
filingDate | 1995-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e04c66845bd0d64faf434f3563eb426c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6a0a9cfefc5a364da87e0cba126b7f89 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_16138324678076211cac4fa7b3ae523b |
publicationDate | 1997-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0954425-A |
titleOfInvention | Lithographic printing plate precursor |
abstract | (57) [Outline] A lithographic printing plate precursor comprising at least a photosensitive hydrophilic swelling layer on a substrate, wherein the hydrophilic swelling layer has a swelling ratio in water of 10 to 1000%, A photosensitive lithographic printing plate precursor having a swelling rate of 5 to 80% with respect to at least one water-soluble organic solvent miscible with water at an arbitrary ratio. [Effect] It is possible to obtain a photosensitive lithographic printing plate precursor having a high ink resilience and a wide control range of dampening water. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1338434-A2 |
priorityDate | 1995-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 463.