http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0953094-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95585944cd76ddfb6dc33ed2a0b84403 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C11D3-37 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-16 |
filingDate | 1995-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1a54b5b2162160048bb97a1c4d934219 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_34e7a372ced343bd5aa3f588b08d361e |
publicationDate | 1997-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0953094-A |
titleOfInvention | Biodegradable builder and method for producing the same |
abstract | (57) [PROBLEMS] To provide an economically advantageous builder having excellent chelating ability and biodegradability, and a method for producing the same. SOLUTION: (a) a saponified product of an acyl vinyl group having a carbon number of 2 to 6 with a saponification rate of 20 to 100 mol%, or (b) a hydroxyl group of the saponified product of 10 to 5 Grafting ratio obtained by graft-copolymerizing an aliphatic carboxylic acid containing one ethylenically unsaturated bond to a modified product obtained by substituting 0 mol% of a methylcarbonylethoxy group and / or a vinylcarbonyloxy group. It is a biodegradable builder comprising a polymer having a weight average molecular weight of 50 to 800% and a number average molecular weight of 10,000 to 500,000. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009035633-A |
priorityDate | 1995-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |