Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_757db2d93afe6d8200b559d9cdb0d06d |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B15-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B23-087 |
filingDate |
1995-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3cb7dc21857330c7b30987b3d32d7804 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3dc1f483651ad178f2090ec8552c242c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0614ca617ed4805334ff6e319cda6efd |
publicationDate |
1997-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H0944943-A |
titleOfInvention |
Magnetic tape guide roller |
abstract |
(57) [Abstract] [PROBLEMS] To improve the oil film formation rate at the contact portion of a magnetic tape guide roller and to prolong the service life. SOLUTION: A large number of minute depression-shaped depressions are randomly formed on the surface of a support pin 1 for supporting a roller 2 made of oil-containing plastic, and an oil film formation rate due to the depressions is improved to prevent abrasion and prolong life. Plan. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013185619-A |
priorityDate |
1995-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |