http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09325457-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-06 |
filingDate | 1996-06-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1b9be7fb56e59b7f5c614fa21152ea6 |
publicationDate | 1997-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09325457-A |
titleOfInvention | Processing method of silver halide photographic material |
abstract | (57) 【Abstract】 PROBLEM TO BE SOLVED: To significantly improve running stability under low replenishment irrespective of the blackening rate or the processing amount of a light-sensitive material, and to run while keeping the generation of black spots and fog low. Provided is a method of processing a light-sensitive material in which the sensitivity fluctuation due to is significantly reduced. SOLUTION: The development start solution and the development replenisher are not the same, and the concentration is 2.5 when processed with the new development start solution. In the case where the sensitivity at a concentration of 2.5 when treated with the developing replenisher in a fresh solution state is 90 to 110%, the bromide content of the developing replenisher is 0.0. 22 mol / l or less Both the development initiation solution and the development replenisher contain 3-pyrazolidones, the content of 3-pyrazolidones in the development replenisher is 1 to 3 times that of the mother liquor, and the development replenishment rate is 200 ml / m. A silver halide photograph characterized by containing 2 to 3 times the amount of an inhibitor that acts by adsorbing on silver and containing a developing replenishing amount of 200 ml / m 2 or less. Achieved by processing the photosensitive material. |
priorityDate | 1996-06-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |