Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f6e960aa6ad2ba6401030159343ebe68 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-00 |
filingDate |
1995-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4db207280447bae19237d33f76fa5af1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b70b2c556b6674a711a1c70abcbe6f1 |
publicationDate |
1997-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H093137-A |
titleOfInvention |
Graft-modified ethylene polymer |
abstract |
(57) [Summary] [Constitution] The density is in the range of 0.850 to 0.980 g / cm 3 , and the melt flow rate (MFR) at 190 ° C. and a load of 2.16 kg is 0.01 to 200 g / 10 min. Within the range, melt tension (MT) and MFR are MT ≦ 2.2 × MFR / 0.84 is satisfied, Mw / Mn is 2.5 or less, and the temperature (Tm) and the density (d) at the maximum peak position in the endothermic curve measured by DSC are Tm <400 × A graft modified ethylene polymer obtained by graft-copolymerizing a polar monomer with an ethylene polymer satisfying the relationship of d-250. [Effect] Excellent adhesion to metal or polar resin. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008024794-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007321026-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007321025-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008156528-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007063196-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1486517-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007262325-A |
priorityDate |
1995-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |