http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09292668-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-31 |
filingDate | 1996-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d94ad33723e7e99181f3feecf2d6d15f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0beb629876860ad1ce9172f662c16e1e |
publicationDate | 1997-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09292668-A |
titleOfInvention | Silver halide photographic material and processing method thereof |
abstract | (57) Abstract: To prevent development unevenness and roller marks (pressure fog or pressure desensitization) even in rapid and / or extremely low replenishment developer processing, and obtain high-sensitivity and high-quality photographic performance. It also improves the drying property. SOLUTION: The amount of coated silver on at least one side of a support is 0.5 g / m 2 or more and 1.5 g / m 2 or less, and the swelling ratio of all hydrophilic colloid layers on the emulsion layer side is 130% or more 200 % Or less, the solubility in water at 25 ° C. is 0.02 A silver halide photographic light-sensitive material comprising a polymer latex containing a monomer unit of 5% by weight or less. |