http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09291466-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F8-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06C29-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06C7-00 |
filingDate | 1996-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4fb37237c960d08bdd0b52508c01d6c5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_72fb75a772adb209e1d80ebb498d2352 |
publicationDate | 1997-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09291466-A |
titleOfInvention | Composite fiber splitting method |
abstract | (57) Abstract: To provide a method for easily dividing a composite fiber formed of a plurality of fiber-forming polymers without performing a splitting with a solvent or the like. SOLUTION: A composite fiber formed of a plurality of fiber-forming polymers having different thermal decomposition rates is 140 to 240 ° C. Of the fiber-forming polymer to thermally decompose at least a part of the polymer having the largest thermal decomposition rate to divide the conjugate fiber. |
priorityDate | 1996-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID415718648 http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID12332 |
Total number of triples: 15.