http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09288324-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-395 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G21K4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-825 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-17 |
filingDate | 1996-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb39a108d2d46d9ec2287cee762172c6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f635d6539a0b3a26fd4a84ad59a6d72 |
publicationDate | 1997-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09288324-A |
titleOfInvention | Silver halide photographic light-sensitive material and combination of silver halide photographic light-sensitive material and radiation intensifying screen |
abstract | (57) Abstract: An X-ray image having sufficient image sensitivity and improved image quality is provided even if replenishment of a developing solution and a fixing solution is small. A photosensitive silver halide emulsion layer is provided on both sides of a support, and the photosensitive silver halide emulsion layer is composed of silver halide grains having a silver chloride content of 15 to 100 mol%. 30% or more of the total projected area of the silver halide grains contained in is a grain having an aspect ratio (equivalent circle diameter / thickness) of 2.0 or more and 25 or less and an average thickness of 0.02 μm or more and 0.35 μm or less. The total coating amount of silver in the emulsion layer is 1.0 to 3.2 g / m 2 on both sides, and the light-sensitive material has the same wavelength as the main emission peak wavelength of the radiation intensifying screen, When exposed and developed with monochromatic light having a half-value width of 15 ± 5 nm and then peeling off the emulsion layer on the side opposite to the exposed surface and measuring the density, the density obtained in the emulsion layer on the exposed surface is the minimum density. The exposure required to obtain a value obtained by adding 0.5 to 0.010 is 0.010. It has a sensitivity of ~ 0.035 lux seconds. |
priorityDate | 1996-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |