http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09286893-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5128cfc84a0fb189fceb3cd240c44493 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-521 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-00 |
filingDate | 1996-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1dd55448cf5c0d276a3b6ac675554f80 |
publicationDate | 1997-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09286893-A |
titleOfInvention | Flame-retardant styrene resin composition with excellent fluidity and heat resistance |
abstract | (57) [Abstract] [PROBLEMS] To provide a flame-retardant styrene-based resin composition having excellent impact resistance, heat resistance, and fluidity, which does not cause mold deposits even after continuous molding for a long period of time. SOLUTION: (A) a rubber-modified styrene resin and (B) A flame-retardant styrene resin composition comprising a flame retardant represented by the following formula (1), and optionally a flame-retardant styrene resin composition containing (C) polyphenylene ether and (D) polyorganosiloxane. To do. Embedded image (In the formula, a, b, and c are 1 to 3, and R 1 , R 2 , and R 3 are Is an aryl group having 6 to 30 carbon atoms. ) |