http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09285826-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_40c1bcb35511762bd1a6c2dd10d52a17 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B21D22-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B21D51-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B21D22-28 |
filingDate | 1996-04-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_898e649aeaa6952d649f6d9f83d1dafb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9528029cab1ef4c90cd8d672049ffaa4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_32676be39aa7052b344c949f1acbde0d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3bd1cf1c2e44797baef8b772d2c92ebd |
publicationDate | 1997-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09285826-A |
titleOfInvention | Squeeze ironing can manufacturing method |
abstract | (57) Abstract: A DI can can be practically manufactured at a squeezing rate of 30% or more by using a precoated plate obtained by coating a metal base plate with a coating material. This eliminates the need for coating after molding, simplifies cleaning, and further improves the Al alloy Alloys other than the 000 series should be used. SOLUTION: As a die for ironing processing in DI processing, an inlet half angle of 3 ° to 20 ° and an outlet half angle of 1 ° to 20 ° Then, the one where the intersection of the inlet half angle and the outlet half angle has a smooth curved surface with a radius of curvature of 0.1 mm or more is used. When there is a bearing portion between the inlet half angle and the outlet half angle, the intersection of the inlet half angle and the bearing portion, and the intersection of the bearing portion and the outlet half angle have a smooth shape with a radius of curvature of 0.1 mm or more. Use a processing die. Furthermore, a volatile lubricating oil is used in the first drawing process. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013039722-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8962538-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015107326-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021193043-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2004072326-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009145338-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009286852-A |
priorityDate | 1996-04-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419584339 http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24461 |
Total number of triples: 24.